The material of your tower packing is decided by three things: the operating temperature, the chemical environment, and the mechanical load. Get any one of them wrong and the packing degrades, contaminates your process, or collapses the bed.
Temperature Limits
- PP (polypropylene) — up to about 100 °C.
- PVDF — up to about 150 °C.
- PTFE — up to about 260 °C.
- Stainless steel — up to 500 °C and beyond, depending on grade.
- Ceramic — 800 °C and above, for high-temperature and corrosive service.
Chemical Compatibility
Plastics resist acids and caustics well, but each has its weaknesses. PP is attacked by strong oxidisers and organic solvents; PVDF handles most acids but not hot strong bases; PTFE is nearly universal but expensive and hard to fabricate. Metals are chosen for strength and temperature, but need a corrosion-resistant grade for acidic duties. Ceramic is the answer when you need both chemical inertness and high-temperature resistance.
Mechanical Strength and Cost
Ceramic has the highest crush strength but is heavier and can break under thermal shock. Metal offers the best strength-to-weight ratio. Plastics are light and inexpensive but creep and soften at elevated temperature.
A Simple Decision Path
- Below 100 °C, aggressive acid or alkali, low cost → PP.
- 100–150 °C or better chemical resistance → PVDF.
- Extreme chemical resistance, higher budget → PTFE.
- High temperature and strength → stainless steel.
- Highest temperature or combined heat + corrosion → ceramic.
XINQUAN supplies random and structured packing in PP, PVDF, PTFE, stainless steel and ceramic. Send us your process conditions for a material recommendation.